回転強度試験における時系列3D scanningと固気液三相の移動解析によるコークス変形が及ぼす充填層内流れ特性評価

Files in This Item:
tetsu 1.pdf5.98 MBPDFView/Open
Please use this identifier to cite or link to this item:http://hdl.handle.net/2115/74849

Title: 回転強度試験における時系列3D scanningと固気液三相の移動解析によるコークス変形が及ぼす充填層内流れ特性評価
Other Titles: Evaluation of Coke Degradation Effect on Flow Characteristics in Packed Bed Using 3D Scanning for Rotational Mechanical Strength Test and Solid-liquid-gas Three-phase Dynamic Model Analysis
Authors: 夏井, 俊悟1 Browse this author →KAKEN DB
澤田, 旺成2 Browse this author
照井, 光輝3 Browse this author
柏原, 佑介4 Browse this author
菊地, 竜也5 Browse this author →KAKEN DB
鈴木, 亮輔6 Browse this author →KAKEN DB
Authors(alt): Natsui, Shungo1
Sawada, Akinori2
Terui, Koki3
Kashihara, Yusuke4
Kikuchi, Tatsuya5
Suzuki, Ryosuke O.6
Keywords: ironmaking blast furnace
coke degradation
molten slag trickle flow
gas permeability
3D scanning
MS-DEM
CLS-SPH
Issue Date: 1-Jul-2018
Publisher: 日本鉄鋼協会
Journal Title: 鉄と鋼
Volume: 104
Issue: 7
Start Page: 347
End Page: 357
Publisher DOI: 10.2355/tetsutohagane.TETSU-2018-005
Abstract: A 3D scanning technique was applied for understanding coke shapes obtained by a rotational strength test, and a numerical dynamic analysis based on the multi-sphere type discrete element method was carried out to clarify the influence of coke degradation on the packed structure. We constructed a trickle flow simulation of molten slag via the smoothed particle hydrodynamics model, and the liquid-gas permeability characteristics exhibited by the coke shapes in the lower part of the blast furnace are discussed accordingly. Coke diameter decreased due to collisions between particles, via the progress of surface- and volume-destruction, and that the particles subsequently became sphere-like in shape. Static holdup of molten slag showed a decreasing tendency with the coke degradation progress, as the void shape and holdup site became spatially uniform as sphericity increased. In the case of packed bed formed by the initial low sphericity or large-sized cokes, the size of the air gap was maintained, although the flow path was non-uniform. Therefore, even if the large amount of holdup did not block the gaseous main flow, in the case of lower coke strength, the sphericity increased due to the deformation progress, and void uniformity could be retained. However, the existence of many narrow void regions remarkably decreased the gas permeability.
Rights: 著作権は日本鉄鋼協会にある
Type: article
URI: http://hdl.handle.net/2115/74849
Appears in Collections:工学院・工学研究院 (Graduate School of Engineering / Faculty of Engineering) > 雑誌発表論文等 (Peer-reviewed Journal Articles, etc)

Submitter: 鈴木 亮輔

Export metadata:

OAI-PMH ( junii2 , jpcoar_1.0 )

MathJax is now OFF:


 

 - Hokkaido University